Hostname: page-component-7b7567c8c-fvjsw Total loading time: 0 Render date: 2026-11-17T18:30:10.398Z Has data issue: false hasContentIssue false

TEM Study of Defects in Laterally Overgrown GaN Layers

Published online by Cambridge University Press:  13 June 2014

J. Park
Affiliation:
Microelectronics Research Center, The University of Texas at Austin, Austin TX 78712-1100
P. A. Grudowski
Affiliation:
Microelectronics Research Center, The University of Texas at Austin, Austin TX 78712-1100
C. J. Eiting
Affiliation:
Microelectronics Research Center, The University of Texas at Austin, Austin TX 78712-1100
R. D. Dupuis
Affiliation:
Microelectronics Research Center, The University of Texas at Austin, Austin TX 78712-1100

Abstract

Transmission electron microscopy was applied to study defects in laterally overgrown GaN layers, with initial growth on Al2O3 substrates followed by further growth over SiO2 masks. Dislocations found in the overgrown areas show changes in line direction. Most dislocations propagate along c-planes. In the overgrown material planar defects (faulted loops) are present on c-planes and their presence is most probably related to segregation of excess point defects and impurities present in this material. They appear to be initiated by the fast lateral growth. Some dislocations with screw orientation become helical resulting from climb motion.

Formation of voids and also a high dislocation density was observed at the boundaries where two overgrowing fronts meet. Tilt and twist components were observed for these boundaries that were different for different overgrown strips grown in the same crystallographic direction suggesting that the GaN subgrain orientations on the two sides of a SiO2 mask are responsible for the final tilt and twist value.

Information

Type
Research Article
Copyright
Copyright © 1999 Materials Research Society
Figure 0

Fig. 1.Cross-section micrographs obtained for the GaN strips grown: (a) along [1 00] and (b) [11 0] directions.

Figure 1

Fig. 2.(a) Cross-section TEM micrograph showing the shape of the overgrown strip near the SiO2 mask edge. Note change of shape from rectangular to the inclined on (1 01); (b) Micrograph showing bending of dislocations close to the SiO2 mask.

Figure 2

Fig. 3.Schematic showing bending of dislocations: (a) in the rectangular and (b) in the triangular shape strips.

Figure 3

Fig. 4.Plan-view micrograph showing: (a) the interface between the homoepitaxial GaN with dislocations at grain boundaries and the area where the overgrowth starts with dislocation lines along the strip length; (b) meeting fronts of two strips showing high dislocation density.

Figure 4

Fig. 5.Defects formed in the overgrown areas: (a) dislocation loops, (b) helical dislocations.

Figure 5

Fig. 6.Cross-section micrograph showing a void and dislocations at the meeting front of two overgrown strips