Hostname: page-component-7b7567c8c-2n9c9 Total loading time: 0 Render date: 2026-11-17T18:59:16.753Z Has data issue: false hasContentIssue false

High Temperature Hardness of Bulk Single Crystal GaN

Published online by Cambridge University Press:  13 June 2014

I. Yonenaga
Affiliation:
Institute for Materials Research, Tohoku University, Sendai 980-8577, Japan
T. Hoshi
Affiliation:
Institute for Materials Research, Tohoku University, Sendai 980-8577, Japan
A. Usui
Affiliation:
Opto-electronics and High Frequency Device Research Laboratories, NEC Corporation, Tsukuba 305-8501, Japan

Abstract

The hardness of single crystal GaN (gallium nitride) at elevated temperature is measured for the first time and compared with other materials. A Vickers indentation method was used to determine the hardness of crack-free GaN samples under an applied load of 0.5N in the temperature range 20 - 1200°C. The hardness is 10.8 GPa at room temperature, which is comparable to that of Si. At elevated temperatures GaN shows higher hardness than Si and GaAs. A high mechanical stability for GaN at high temperature is deduced.

Information

Type
Research Article
Copyright
Copyright © 1996 Materials Research Society
Figure 0

Figure 1.Optical micrograph of Vickers indent of bulk single crystal GaN (a) at RT with an applied load of 1 N and dwell time of 30 s and (b) at 200°C with 0.5 N and 30 s.

Figure 1

Figure 2.Vickers hardness of bulk single crystal GaN plotted against reciprocal temperature, with an applied load of 0.5 N and dwell time of 30 s, together with those of Si, GaAs, and 6H-SiC. The hardness of sapphire obtained with 2 N and 15 s is superimposed [10].

Figure 2

Table I.Vickers hardness of GaN and various semiconductors at room temperature or 300°C with an applied load of 0.5 N and dwell time of 30 s. The hardness of sapphire obtained with 2 N and 15 s is also included [10].