Hostname: page-component-7b7567c8c-wxvwp Total loading time: 0 Render date: 2026-11-17T19:49:06.710Z Has data issue: false hasContentIssue false

Transport, Growth Mechanisms, and Material Quality in GaN Epitaxial Lateral Overgrowth

Published online by Cambridge University Press:  13 June 2014

Albert G. Baca
Affiliation:
Sandia National Laboratories, Albuquerque, NM 87185

Abstract

Growth kinetics, mechanisms, and material quality in GaN epitaxial lateral over-growth (ELO) were examined using a single mask of systematically varied patterns. A 2-D gas phase reaction/diffusion model describes how transport of the Ga precursor to the growth surface enhances the lateral rate in the early stages of growth. In agreement with SEM studies of truncated growth runs, the model also predicts the dramatic decrease in the lateral rate that occurs as GaN over-growth reduces the exposed area of the mask. At the point of convergence, a step-flow coalescence mechanism is observed to fill in the area between lateral growth-fronts. This alternative growth mode in which a secondary growth of GaN is nucleated along a single convergence line, may be responsible for producing smooth films observed to have uniform cathodoluminescence (CL) when using 1μm nucleation zones. Although emission is comprised of both UV (∼365nm) and yellow (∼550nm) components, the spectra suggest these films have reduced concentrations of threading dislocations normally associated with non-radiative recombination centers and defects known to accompany growth-front convergence lines.

Information

Type
Research Article
Copyright
Copyright © 1999 Materials Research Society
Figure 0

Figure 1.Growth rate g (normalized by the unenhanced growth rate go) calculated by the 2-D transport model as a function of fill-factor θ. Solid line shows the fit from Eq. (3).

Figure 1

Figure 2.SEM micrographs showing the extent of lateral overgrowth from patterns of different masked dimensions (a) 1:32 (×600 magnification), (b) 1:16 (×1000), (c) 1:8 (×1600)

Figure 2

Figure 3.Comparison of lateral growth distance as a function of initial fill-factor measured from the SEM micrographs and calculated from Eq. (5).

Figure 3

Figure 4.(a) SEM of a selective area growth dot pattern showing that adjacent lateral growth fronts have only just touched. (b) Diagram of the step-flow coalescence mechanism.

Figure 4

Figure 5.(a) CL image at 363 nm of non-ELO GaN (4 μm grown at 1050°C). (b) CL image of ELO GaN from a 1:1 pattern (4 μm grown at 1050°C).