Hostname: page-component-7b7567c8c-wxvwp Total loading time: 0 Render date: 2026-11-17T09:42:30.630Z Has data issue: false hasContentIssue false

Ranges of Deposition Temperatures Applicable for Metalorganic Vapor Phase Epitaxy of Gan Films Via the Technique of Pendeo-Epitaxy

Published online by Cambridge University Press:  13 June 2014

D. B. Thomson
Affiliation:
Department of Materials Science and Engineering, North Carolina State University, Box 7907, Raleigh, NC 27695-7907
T. Gehrke
Affiliation:
Department of Materials Science and Engineering, North Carolina State University, Box 7907, Raleigh, NC 27695-7907
K. J. Linthicum
Affiliation:
Department of Materials Science and Engineering, North Carolina State University, Box 7907, Raleigh, NC 27695-7907
P. Rajagopal
Affiliation:
Department of Materials Science and Engineering, North Carolina State University, Box 7907, Raleigh, NC 27695-7907
R. F. Davis
Affiliation:
Department of Materials Science and Engineering, North Carolina State University, Box 7907, Raleigh, NC 27695-7907

Abstract

Pendeo-epitaxy is a type of selective growth of thin films from the sidewalls of etched forms. The resulting films are suspended from the sidewalls and do not interface with the substrate. This process route has advantages over conventional lateral epitaxial overgrowth (LEO) techniques. In this research, pendeo-epitaxial growth of GaN films has been achieved on elongated GaN seed columns. The seed columns were etched from GaN grown on 6H-SiC (0001) substrates via metalorganic vapor phase epitaxy (MOVPE). Silicon nitride mask layers atop the GaN seed columns forced growth from the sidewalls. Pendeo-epitaxial growth of GaN was investigated using several growth temperatures. Higher growth temperatures resulted in improved coalescence due to greater lateral to vertical growth ratios.

Information

Type
Research Article
Copyright
Copyright © 1999 Materials Research Society
Figure 0

Figure 1.Schematic diagram showing the process steps for growth of pendeo-epitaxial GaN: (a) GaN seed layer, (b) etched GaN columns prior to PE growth, (c) partial growth of PE GaN showing growth only from the sidewalls, (d) coalesced growth of PE GaN.

Figure 1

Figure 2Cross-sectional SEM micrographs of PE GaN grown at 1000°C for (a) 30 minutes, and (b) 80 minutes.

Figure 2

Figure 3Plan view SEM micrographs of PE GaN grown for 80 minutes at temperatures of: (a) 1000°C, (b) 1050°C, and (c) 1080°C.

Figure 3

Figure 4Cross-sectional SEM micrographs of PE GaN grown at 1080°C for 80 minutes showing features at (a) low magnification and (b) high magnification.