Hostname: page-component-7b7567c8c-w7t8q Total loading time: 0 Render date: 2026-11-18T19:27:44.281Z Has data issue: false hasContentIssue false

Fabrication of Smooth GaN-Based Laser Facets

Published online by Cambridge University Press:  13 June 2014

D. A. Stocker
Affiliation:
Center for Photonics Research, Boston University, Boston, MA 02215
E. F. Schubert
Affiliation:
Center for Photonics Research, Boston University, Boston, MA 02215
K. S. Boutros
Affiliation:
Epitronics, Phoenix, AZ 85027
J. M. Redwing
Affiliation:
Epitronics, Phoenix, AZ 85027

Abstract

A method is presented for fabricating fully wet-etched InGaN/GaN laser cavities using hotoenhanced electrochemical wet etching followed by crystallographic wet etching. Crystallographic wet chemical etching of n- and p-type GaN grown on c-plane sapphire is achieved using H3PO4 and various hydroxides, with etch rates as high as 3.2.μm/min. The crystallographic GaN etch planes are {0001}, {100}, {10 }, {10 }, and {103}. The vertical {100} planes appear perfectly smooth when viewed with a field-effect scanning electron microscope (FESEM), indicating a surface roughness less than 5 nm, suitable for laser facets. The etch rate and crystallographic nature for the various etching solutions are independent of conductivity, as shown by seamless etching of a p-GaN/undoped, high-resistivity GaN homojunction.

Information

Type
Research Article
Copyright
Copyright © 1999 Materials Research Society
Figure 0

Table I:Etch rates and observed etching planes for various chemicals

Figure 1

FIG. 1:High-resolution field-effect SEM image of a vertical {10 0 } plane etched in n-GaN by KOH dissolved in ethylene glycol at a temperature of 170°C.

Figure 2

FIG. 2:SEM image of a {10 0 } surface made by crystallographic wet etching in molten KOH at 195°C. The upper portion of the epilayer is p-GaN, while the lower 1 μm is highly resistive GaN.

Figure 3

FIG. 3:Smoothing of a surface produced by photo-enhanced electrochemical (PEC) etching of an InGaN/GaN double heterostructure. The 10 μm bar underneath the figure is valid for all of the SEM images. (a) PEC-etched surface before smoothing by crystallographic etching in molten KOH at 175°C. (b) PEC-etched surface after smoothing for 1 min. (c) After smoothing for 3 min. (d) After smoothing for 9 min.