Mg Segregation, Difficulties of P-Doping in GaN

Published online by Cambridge University Press:  13 June 2014

I. Grzegory
Affiliation:
High Pressure Research Center “Unipress,” Polish Academy of Sciences, Warsaw, Poland
S. Porowski
Affiliation:
High Pressure Research Center “Unipress,” Polish Academy of Sciences, Warsaw, Poland
R.D. Dupuis
Affiliation:
The University of Texas at Austin, Microelectronics Research Center, PRC/MER 1.606D-R9900, Austin TX 78712-1100 USA
C.J. Eiting
Affiliation:
The University of Texas at Austin, Microelectronics Research Center, PRC/MER 1.606D-R9900, Austin TX 78712-1100 USA

Abstract

Transmission electron microscopy has been used to study defects formed in Mg-doped GaN crystals. Three types of crystals have been studied: bulk crystals grown by a high pressure and high temperature process with Mg added to the Ga solution and two types of crystals grown by metal-organic chemical vapor deposition (MOCVD) where Mg was either delta-doped or continuously doped. Spontaneous ordering was observed in bulk crystals. The ordering consists of Mg rich planar defects on basal planes separated by 10.4 nm and occurs only for growth in the N to Ga polar direction (000 N polarity). These planar defects exhibit the characteristics of stacking faults with a shift vector of a 1/3 [1 00] +c/2 but some other features identify these defects as inversion domains. Different type of defects were formed on the opposite site of the crystal (Ga to N polar direction), where the growth rate is also an order of magnitude faster compared to the growth with N-polarity. These defects are three-dimensional: pyramidal and rectangular, empty inside with Mg segregation on internal surfaces. The same types of defects seen for the two growth polarities in the bulk crystals were also observed in the MOCVD grown GaN samples with Mg delta doping, but were not observed in the crystals where Mg was added continuously.

Information

Type
Research Article
Copyright
Copyright © 1996 Materials Research Society
Figure 0

Fig. 1.(a) High magnification of sub-surface area, grown in the N polar directionindicated by ball model shown in (b), showing periodic arrangement of planar defects; (c) fraction of the diffraction pattern between (1 00) and (1 01) diffraction spots showing formation of satellite spots due to formation of ordered structure; (d) intensity distribution through this pattern showing division of (0001) reciprocal distance into 20 equal spacings; (e) A splitting of (0001) reflection.

Figure 1

Fig. 2.(a) Tetrahedral-shaped defects formed in bulk GaN crystals grown with Ga polarity, (b) Fraction of the diffraction pattern between (1 00) and (1 01) diffraction spots obtained from this area of the crystal. Note lack of satellite spots; (c) Defects observed in plan-view configuration indicating that they are empty inside; (d) Another type of hollow defect (in cross-section) formed for growth with Ga polarity.

Figure 2

Fig. 3.(a) Cross-section micrograph from the MOCVD grown GaN sample with Mg-delta doping. Note high density of triangular and also rectangular defects typical for growth with Ga polarity. The arrows show the area where planar defects are formed typical for N polarity. Their higher magnification of the area with planar defects is shown in (b).

Figure 3

Fig. 4.(a) SIMS measurements obtained from a MOCVD sample with Mg delta doping. A higher Mg concentration was measured in the area where planar defects were formed, similar to those observed in the bulk GaN:Mg, (b) Similar analysis for the sample with continuous Mg doping where formation of structural defects was not observed despite the comparable Mg concentration.