Hostname: page-component-7b7567c8c-fvjsw Total loading time: 0 Render date: 2026-11-16T16:20:43.158Z Has data issue: false hasContentIssue false

Formation and stability of the prismatic stacking faultin wurtzite (Al,Ga,In) nitrides

Published online by Cambridge University Press:  13 June 2014

P. Ruterana*
Affiliation:
Laboratoire d’Etudes et de Recherches sur les Matériaux –Institut des Sciences de la Matière et du Rayonnement, UPRESA-CNRS 6004, 6 Bd Maréchal Juin, 14050 Caen Cedex, France
A. Béré
Affiliation:
Laboratoire d’Etudes et de Recherches sur les Matériaux –Institut des Sciences de la Matière et du Rayonnement, UPRESA-CNRS 6004, 6 Bd Maréchal Juin, 14050 Caen Cedex, France
G. Nouet
Affiliation:
Laboratoire d’Etudes et de Recherches sur les Matériaux –Institut des Sciences de la Matière et du Rayonnement, UPRESA-CNRS 6004, 6 Bd Maréchal Juin, 14050 Caen Cedex, France
*
1Author for correspondance: email : ruterana@lermat8.ismra.fr, Tel: 33 2 31 45 26 53, Fax: 33 2 31 45 26 60

Abstract

The formation of the {1 10} stacking fault, which has two atomic configurations in wurtzite (Ga,Al,In)N, has been investigated by high resolution electron microscopy and energetic calculations. It originates from steps at the SiC surface and it can form on a flat (0001) sapphire surface. A modified Stillinger-Weber potential was used in order to investigate the relative stability of the two atomic configurations. They have comparable energy in AlN, whereas the 1/2<10 1>{1 10} configuration is more stable in GaN and InN. In GaN layers, only the 1/2<10 1>{1 10} configuration was observed. The 1/6<20 3> configuration was found in small areas inside the AlN buffer layer where it folded rapidly to the basal plane, and when back into the prismatic plane, it took the 1/2<10 1>{1 10} atomic configuration.

Information

Type
Research Article
Copyright
Copyright © 1996 Materials Research Society
Figure 0

Figure 1.Atomic configurations of the { 110 }stacking fault seen along [0001], a) The ½ [ 101 ] displacement vector, b) The 1/6 [ 203 ] stacking fault

Figure 1

Figure 2.Generation of a prismatic stacking fault on a I1 type of step on the (0001) surface of 6H-SiC

Figure 2

Table 1.Type of defects forming at an interface step between 2H-GaN and 6H-SiC

Figure 3

Table 2.Residual translation in GaN as a function of the step height in Al2O3

Figure 4

Figure3.Four of the 8 possible stacking of wurtzite (Ga,Al)N on the (0001) sapphire surface, the polyhedra configurations at the interface are shown

Figure 5

Table 3.Formation energy in me V/2 for the relaxed atomic configurations of the {110 } prismatic stacking fault, in parenthesis are the values of reference 23