Hostname: page-component-7b7567c8c-48dgx Total loading time: 0 Render date: 2026-11-17T21:27:37.638Z Has data issue: false hasContentIssue false

Emission at 247 nm from GaN quantum wells grown by MOCVD

Published online by Cambridge University Press:  13 June 2014

Takao Someya
Affiliation:
Research Center for Advanced Science and Technology, University of Tokyo, 4-6-1 Komaba, Meguro-ku, Tokyo 153-8904, Japan, Institute of Industrial Science, University of Tokyo, 7-22-1 Roppongi, Minato-ku, Tokyo 106-8558, Japan
Katsuyuki Hoshino
Affiliation:
Research Center for Advanced Science and Technology, University of Tokyo, 4-6-1 Komaba, Meguro-ku, Tokyo 153-8904, Japan, Institute of Industrial Science, University of Tokyo, 7-22-1 Roppongi, Minato-ku, Tokyo 106-8558, Japan
Janet C. Harris
Affiliation:
Research Center for Advanced Science and Technology, University of Tokyo, 4-6-1 Komaba, Meguro-ku, Tokyo 153-8904, Japan, Institute of Industrial Science, University of Tokyo, 7-22-1 Roppongi, Minato-ku, Tokyo 106-8558, Japan
Koichi Tachibana
Affiliation:
Research Center for Advanced Science and Technology, University of Tokyo, 4-6-1 Komaba, Meguro-ku, Tokyo 153-8904, Japan, Institute of Industrial Science, University of Tokyo, 7-22-1 Roppongi, Minato-ku, Tokyo 106-8558, Japan
Satoshi Kako
Affiliation:
Research Center for Advanced Science and Technology, University of Tokyo, 4-6-1 Komaba, Meguro-ku, Tokyo 153-8904, Japan, Institute of Industrial Science, University of Tokyo, 7-22-1 Roppongi, Minato-ku, Tokyo 106-8558, Japan
Yasuhiko Arakawa
Affiliation:
Research Center for Advanced Science and Technology, University of Tokyo, 4-6-1 Komaba, Meguro-ku, Tokyo 153-8904, Japan, Institute of Industrial Science, University of Tokyo, 7-22-1 Roppongi, Minato-ku, Tokyo 106-8558, Japan

Abstract

Photoluminescence (PL) spectra were measured at room temperature for GaN quantum wells (QWs) with Al0.8Ga0.2N barriers, which were grown by atmospheric-pressure metal organic chemical vapor deposition (MOCVD). The thickness of the GaN QW layers was systematically varied from one monolayer to four monolayers. We clearly observed a PL peak at a wavelength as short as 247 nm (5.03 eV) from one monolayer-thick QWs. The effective confinement energy is as large as 1.63 eV.

Information

Type
Research Article
Copyright
Copyright © 1996 Materials Research Society
Figure 0

Figure 1Photoluminescence spectra for GaN quantum wells, whose thicknesses are from one monolayer to three monolayers, measured at room temperature.

Figure 1

Figure 2Peak wavelength in photoluminescence spectra is plotted as a function of the thickness of GaN well layers.