Hostname: page-component-7b7567c8c-wxvwp Total loading time: 0 Render date: 2026-11-18T11:05:39.429Z Has data issue: false hasContentIssue false

Focused Ion Beam Etching of GaN

Published online by Cambridge University Press:  13 June 2014

C. Flierl
Affiliation:
Department of Electrical and Electronic Engineering, University of Bristol, Bristol BS8 1TR, UNITED KINGDOM;
I.H. White
Affiliation:
Department of Electrical and Electronic Engineering, University of Bristol, Bristol BS8 1TR, UNITED KINGDOM;
M. Kuball
Affiliation:
H.H. Wills Physics Laboratory, University of Bristol, Bristol BS8 1TL, UNITED KINGDOM
P.J. Heard
Affiliation:
Interface Analysis Centre, University of Bristol, Bristol BS2 8BS, UNITED KINGDOM
G.C. Allen
Affiliation:
Interface Analysis Centre, University of Bristol, Bristol BS2 8BS, UNITED KINGDOM
C. Marinelli
Affiliation:
Department of Electrical and Electronic Engineering, University of Bristol, Bristol BS8 1TR, UNITED KINGDOM;
J.M. Rorison
Affiliation:
Department of Electrical and Electronic Engineering, University of Bristol, Bristol BS8 1TR, UNITED KINGDOM;
R.V. Penty
Affiliation:
Department of Electrical and Electronic Engineering, University of Bristol, Bristol BS8 1TR, UNITED KINGDOM;
Y. Chen
Affiliation:
Hewlett-Packard Laboratories, Palo Alto CA 94304, USA
S.Y. Wang
Affiliation:
Hewlett-Packard Laboratories, Palo Alto CA 94304, USA

Abstract

We have investigated the use of focused ion beam (FIB) etching for the fabrication of GaN-based devices. Although work has shown that conventional reactive ion etching (RIE) is in most cases appropriate for the GaN device fabrication, the direct write facility of FIB etching – a well-established technique for optical mask repair and for IC failure analysis and repair – without the requirement for depositing an etch mask is invaluable. A gallium ion beam of about 20nm diameter was used to sputter GaN material. The etching rate depends linearly on the ion dose per area with a slope of 3.5 × 10−4 μm3/pC. At a current of 3nA, for example, this corresponds to an each rate of 1.05 μm3/s. Good etching qualities have been achieved with a side wall roughness significantly below 0.1 μm. Change in the roughness of the etched surface plane stay below 8nm.

Information

Type
Research Article
Copyright
Copyright © 1999 Materials Research Society
Figure 0

Figure 1:Focused ion beam (FIB)-etched pattern in GaN layer, fabricated using Ga-ion doses of (a) 500, (b,d) 1000, (c) 1500, and (e) 2000pC/μm2

Figure 1

Figure 2:Atomic force microscopy (AFM) image of FIB-etched structure in GaN.

Figure 2

Figure 3:Etch rate as function of gallium ion dose.

Figure 3

Figure 4:Change in the root mean square (RMS) of the GaN surface roughness after the FIB etching.

Figure 4

Figure 5:Scanning electron microscopy images of FIB-etched edge.