Emission Enhancement of GaN/AlGaN Single-Quantum-Wells Due to Screening of Piezoelectric Field

Published online by Cambridge University Press:  13 June 2014

A. Kinoshita
Affiliation:
The Institute of Physical and Chemical Research (RIKEN), Hirosawa 2-1, Wako-shi, Saitama, 351-0198, Japan
H. Hirayama
Affiliation:
The Institute of Physical and Chemical Research (RIKEN), Hirosawa 2-1, Wako-shi, Saitama, 351-0198, Japan
P. Riblet
Affiliation:
The Institute of Physical and Chemical Research (RIKEN), Hirosawa 2-1, Wako-shi, Saitama, 351-0198, Japan
M. Ainoya
Affiliation:
The Institute of Physical and Chemical Research (RIKEN), Hirosawa 2-1, Wako-shi, Saitama, 351-0198, JapanDepartment of Chemical Engineering, Waseda University, Okubo 3-4-1, Shinjuku-ku, Tokyo, 169-8555, Japan
A. Hirata
Affiliation:
Department of Chemical Engineering, Waseda University, Okubo 3-4-1, Shinjuku-ku, Tokyo, 169-8555, Japan
Y. Aoyagi
Affiliation:
The Institute of Physical and Chemical Research (RIKEN), Hirosawa 2-1, Wako-shi, Saitama, 351-0198, Japan

Abstract

Photoluminescence (PL) enhancement due to the screening of piezoelectric field induced by Si-doping is systematically studied in GaN/AlGaN quantum wells (QWs) fabricated by metal organic vapor-phase-epitaxy (MOVPE). The PL enhancement ratio of QWs for Si-doped directly into the wells was much larger than that for doped only into the barrier layers. This result shows that the crystal quality of the quantum well is not so damaged by heavy Si-doping, which is different from the cases of GaAs or InP material systems. The PL intensity enhancement ratio was especially large for thick wells. The typical value of the enhancement ratio was 30 times for a 5 nm-thick single QW. The optimum Si-doping concentration was approximately 4×1018 cm−3. From the well width dependence of the PL enhancement ratio and PL peak shift under high excitation conditions, we determined that the dominant effect inducing the PL enhancement is screening of piezoelectric field in the QWs. These results indicate that Si-doping is very effective for the application of GaN/AlGaN QWs to optical devices.

Information

Type
Research Article
Copyright
Copyright © 1996 Materials Research Society
Figure 0

Figure 1.PL spectra of undoped GaN/Al0.16Ga0.84N 5MQWs with various well width measured at 77K. The PL peak energy and intensity strongly depend on the well width.

Figure 1

Figure 2.PL intensity enhancement ratio for Si-doped GaN/Al0.16Ga0.84N 5MQWs as a function of Si-doping concentration. Si is doped in the wells or barriers. The well and barrier width were 4nm and 6nm, respectivery.

Figure 2

Figure 3.PL intensity enhancement ratio for Si-doped GaN/Al0.14Ga0.86N SQWs with various well width as a function of Si-doping concentration.

Figure 3

Figure 4.PL peak energy shift for Si-doped GaN/Al0.14Ga0.86N SQWs with various well width as a function of Si-doping concentration.

Figure 4

Figure 5.PL peak energy difference between high and low excitation conditions for undoped and Si-doped GaN/Al0.14Ga0.86N SQWs as a function of well width. Si-doping concentration was 1.8×1018 cm−3.