Hostname: page-component-7b7567c8c-w7t8q Total loading time: 0 Render date: 2026-11-17T22:49:17.623Z Has data issue: false hasContentIssue false

Electrical Characterization of MOVPE-Grown P-Type GaN:Mg Against Annealing Temperature

Published online by Cambridge University Press:  13 June 2014

Abstract

Hall effect measurements have been applied for the electrical characterization of p-type Mg-doped GaN grown by metalorganic vapor-phase epitaxy on sapphire substrates in terms of annealing temperature for dehydrogenation (N2 annealing) and hydrogenation (H2 annealing) of the acceptors. With the N2 annealing temperature from 600 to 900 °C for dehydrogenation, both hole concentration and mobility increases, showing more activation of acceptors and less incorporation of unfavorable scattering centers probably originating from Mg-H bondings. The N2 annealing at higher than the growth temperature results in reduced hole concentration, but the mobility gets higher. Some defects compensating acceptors may be induced at high temperature annealing, but they seem to be no scattering centers and be inactivated by successive hydrogenation and re-dehydrogenation at the optimum dehydrogenation temperature 900 °C. The electrical degradation of GaN due to thermal damage is not very destructive and can be well recovered by annealing treatments.

Information

Type
Research Article
Copyright
Copyright © 1999 Materials Research Society
Figure 0

Fig. 1Temperature dependence of hole concentration and hole Hall mobility of GaN:Mg samples subjected to different dehydrogenation (N2 annealing) temperature.

Figure 1

Fig. 224 K PL spectra of GaN:Mg samples subjected to different dehydrogenation (N2 annealing temperature.

Figure 2

Fig. 3Variation of hole concentration at RT after dehydrogenation (N2 annealing) and successive hydrogenation(H2 annealing) against the dehydrogenation temperature. The hydrogenation was done at the same condition, 700 °C and 20 min.

Figure 3

Fig. 4Temperature dependence of hole concentration and hole Hall mobility of GaN:Mg samples experienced dehydrogenation, hydrogenation, and redehydrogenation, successively. The 1st dehydrogenation temperatures are shown as a parameter and the succesive hydrogenation and re-dehydrogenation were done at 700 °C and 900 °C, respectively.