Hostname: page-component-7b7567c8c-2n9c9 Total loading time: 0 Render date: 2026-11-18T02:11:07.831Z Has data issue: false hasContentIssue false

Photoluminescence and Cathodoluminescence of GaN doped with Pr

Published online by Cambridge University Press:  13 June 2014

H. J. Lozykowski*
Affiliation:
School of Electrical Engineering & Computer Science, and Condensed Matter & Surface
W. M. Jadwisienczak
Affiliation:
Sciences Program, Ohio University, Stocker Center, Athens, OH, 45701
I. Brown
Affiliation:
Lawrence Berkeley Laboratory, University of California Berkeley, Berkeley, California 94720
*
1Electronic address: lozykows@bobcat.ent.ohiou.edu

Abstract

In this paper we have reported the observation of visible photoluminescence (PL) and cathodoluminescence (CL) of Pr implanted in GaN. The implanted samples were given isochronal thermal annealing treatments at a temperature of 11000 C in NH3, N2, Ar2, and in forming gas N2 +H2, at atmospheric pressure to recover implantation damages and activate the rare earth ions. The sharp characteristic emission lines corresponding to Pr3+ intra-4fn -shell transitions are resolved in the spectral range from 350 nm to 1150 nm, and observed over the temperature range of 12 K-335 K. The PL and CL decay kinetics measurement was performed for 3P1, 3P0 and 1D2 levels.

Information

Type
Research Article
Copyright
Copyright © 1996 Materials Research Society
Figure 0

Fig.1CL (a) and PL (b) spectra of GaN: Pr3+ recorded at 13 K and 330 K Inserts show magnified lower intensity emission lines of CL (a) and PL (b) spectra respectively. Numbers refer to transitions assignment from Fig. 1a.

Figure 1

Fig.2PL spectra of GaN: Pr3+ annealed at 11000° C during 1h in NH3, N2, Ar2, and in forming gas

Figure 2

Fig.3The PL intensity of GaN: Pr3+ annealed at 11000 C during 1h in NH3, N2, Ar2, monitored <$>

Figure 3

Fig. 4Luminescence decay observed from GaN: Pr3+ after N2 laser pulse exc. (PL) and electron pulse exc. (CL) at 653 nm. Inset shows temperature dependence of 3P0 decay time (■ ●) fitted to Eq.1 (doted, solid lines).

Figure 4

TABLE 1.CL and PL decay times of GaN:Pr3+