Amplification Path Length Dependence Studies of Stimulated Emission from Optically Pumped InGaN/GaN Multiple Quantum Wells

Published online by Cambridge University Press:  13 June 2014

T.J. Schmidt
Affiliation:
Center for Laser and Photonics Research and Dept. of Physics Oklahoma State University, Stillwater, OK 74078
S. Bidnyk
Affiliation:
Center for Laser and Photonics Research and Dept. of Physics Oklahoma State University, Stillwater, OK 74078
Yong-Hoon Cho
Affiliation:
Center for Laser and Photonics Research and Dept. of Physics Oklahoma State University, Stillwater, OK 74078
A.J. Fischer
Affiliation:
Center for Laser and Photonics Research and Dept. of Physics Oklahoma State University, Stillwater, OK 74078
J.J. Song
Affiliation:
Center for Laser and Photonics Research and Dept. of Physics Oklahoma State University, Stillwater, OK 74078
S. Keller
Affiliation:
Electrical and Computer Engineering and Materials Depts. University of California, Santa Barbara, CA 93106
U.K. Mishra
Affiliation:
Electrical and Computer Engineering and Materials Depts. University of California, Santa Barbara, CA 93106
S.P. DenBaars
Affiliation:
Electrical and Computer Engineering and Materials Depts. University of California, Santa Barbara, CA 93106

Abstract

Optically pumped stimulated emission (SE) from InGaN/GaN multiple quantum wells (MQWs) grown by metalorganic chemical vapor deposition has been systematically studied as a function of excitation length (Lexc). Two distinct SE peaks were observed from these structures: one that originates at 425 nm at 10 K (430 nm at 300 K) and another that originates at 434 nm at 10 K (438 nm at 300 K). The SE threshold for the high energy peak was observed to always be lower than that of the low energy peak, but the difference was found to decrease greatly with increasing Lexc. A detailed study of the emission intensity of these two SE peaks as a function of excitation density shows that the two peaks compete for gain in the MQW active region.

Information

Type
Research Article
Copyright
Copyright © 1999 Materials Research Society
Figure 0

Figure 1:10 K stimulated emission spectra (solid lines) from an InGaN/GaN MQW subjected to several excitation densities, where Io = 100 kW/cm2. The low power PL (dashed line) and PLE (dotted line) spectra are also shown for comparison. The SE spectra have been normalized and displaced vertically for clarity.

Figure 1

Figure 2:Stimulated emission spectra of SE peak (1) at (a) 200 K, (b) 300 K, and (c) 450 K illustrating SE peak (1) is composed of a multitude of narrow (< G6.54.1 nm) stimulated emission peaks that do not noticeably broaden with increasing temperature. The SE spectra shown were collected for excitation densities twice the SE threshold for the respective temperatures. The spontaneous emission spectra (dotted lines) are also shown for excitation densities half that of the SE threshold at each temperature. The SE spectra have been normalized for clarity.

Figure 2

Figure 3:(a) Stimulated emission threshold as a function of excitation length for SE peaks (1) and (2) at 10 K. (b) Peak position of SE peaks (1) and (2) as a function of excitation length at 10 K. The insets show the behavior observed at room temperature. The solid lines are given only as guides for the eye.

Figure 3

Figure 4:10 K modal gain spectra of an InGaN/GaN MQW at several excitation densities. The excitation densities are given with respect to the SE threshold measured for long (∼ 2.5 mm) excitation lengths.

Figure 4

Figure 5:Emission intensity of SE peaks (1) and (2) as a function of optical excitation density at 10 K, illustrating gain competition. The excitation length is 1300 μm. The respective SE thresholds, Ith, of SE peaks (1) and (2) are indicated for completeness. The solid lines are given only as guides for the eye.