Abstract

We report both the device fabrication and characterization of InGaN/GaN single quantum well LEDs grown on sapphire substrates using multi-wafer MOVPE reactor. To improve current spreading of the LEDs, a self-aligned process is developed to define LED mesa that is coated with a thin, semi-transparent Ni/Au (40 Å/40 Å) layer. A detailed study on the ohmic contact resistance of Ni/Cr/Au on p-GaN versus annealing temperatures is carried out on transmission line test structures. It was found that the annealing temperatures between 300 to 500 °C yield the lowest specific contact resistance rc ( 0.016 Ω-cm2 at a current density of 66.7 mA/cm). Based on the extracted rc from the transmission line measurement, we estimate that the contact resistance of the p-type GaN accounts for ∼ 88% of the total series resistance of the LED.

Information

Type
Research Article
Copyright
Copyright © 1999 Materials Research Society
Figure 0

Fig. 1(a)The schematics of self-aligned InGaN/GaN LED structure. Note that a thin Ni/Au layer is deposited on top of the LED mesa to improve the current spreading.

Figure 1

Fig. 1(b)SEM of a typical LED structure with a magnified view of the edges of mesa after RIE etching.

Figure 2

Fig. 2Thickness uniformity across the diameter of a 2-inch LED wafer. A typical reflectance spectrum is also shown here.

Figure 3

Fig 3(a) The I-V of the LED with and without the current spreading layer; and (b) the emission spectrum of the LED.

Figure 4

Fig. 4The measured resistance versus spacing of the TL test pattern at two different measurement currents.

Figure 5

Fig. 5The extracted rc measured at different current levels and annealing temperatures. The width of the rectangular TL pattern is 300 μm.