Control of the Polarity and Surface Morphology of GaN Films Deposited on C-Plane Sapphire

Published online by Cambridge University Press:  13 June 2014

M. Sumiya
Affiliation:
Department of Electrical and Electronic Engineering, Shizuoka University, 3-5-1 Johoku Hamamatsu, 432-8561, Japan
T. Ohnishi
Affiliation:
Materials and Structures Laboratory,
A. Ohtomo
Affiliation:
Department of Innovative and Engineering Materials, Tokyo Institute of Technology, 4259 Nagatsuta Yokohama, 226-8502, Japan
M. Kawasaki
Affiliation:
Department of Innovative and Engineering Materials, Tokyo Institute of Technology, 4259 Nagatsuta Yokohama, 226-8502, Japan
M. Yoshimoto
Affiliation:
Materials and Structures Laboratory,
H. Koinuma
Affiliation:
Materials and Structures Laboratory,
K. Ohtsuka
Affiliation:
Research and Development Division, Sanken Electric Co. Ltd., 3-6-3 Kitano Niiza, 352-8666, Japan

Abstract

Control of the polarity of GaN films deposited by metalorganic chemical vapor deposition was achieved by substrate nitridation and subsequent annealing of a buffer layer. The surface morphology and optical properties of 1.2μm GaN films were influenced by the different growth mode due to the polar direction. Coaxial impact collision ion scattering spectroscopy revealed that the polarity composition of a buffer layer on nitrided sapphire varied by annealing in a H2 atmosphere. It was considered that the systematic variation of the surface morphology was caused by the polarity composition of the buffer layer.

Information

Type
Research Article
Copyright
Copyright © 1999 Materials Research Society
Figure 0

Fig.1Schematic illustration of wrutzite GaN structure oriented along c-axis. Left side is (0001) Ga-face which is defined +c. Right side is (0001) N-face which is defined which is defined −c.

Figure 1

Fig.2Surface morphology of GaN films deposited on the buffer layer whose polarity was controlled by the annealing time of (a) 30min, (b)40min, (c)60min and – (d) 100min. GaN epilayers were deposited

Figure 2

Fig. 3PL spectra near band edge at 10K for +c and −c GaN films on (a) 20nm buffer layer, (b)160nm buffer layer annealed for 10min. (c) GaN on 20nm buffer and (d) 160nm buffer layer annealed for 60min. The substrate was nitrided in (b)-(d).

Figure 3

Fig. 4CAICISS spectra of 160nm buffer layers on a nitrided sapphire for (b) 20min and (c) 30min. The lines in (b) and (c) are calculated line from the weight mean of the spectra of (a) +c and (d) −c ZnO (See the text).

Figure 4

Fig. 5Schematic illustration of the variation of buffer layer on a nitrided sapphire by the annealing. The annealing should enhanced the etching. (a) as-deposited buffer layer covered with +c changed to the buffer layer with (c) −c polarity through the transition (b). as illustrated in Fig.5.

Figure 5

Fig. 6Ratio of flat hexagonal fact of GaN films deposited on 160nm buffer layer annealed for up to 100min. The sapphire was nitrided. The values of crystal structure for those films and GaN film on 20nm buffer layer as a reference are also plotted.