Summary

Before discussing the interpretation of polymer spectra it is important to consider two factors which may cause problems. These are sample charging, with the associated problem of binding energy scale referencing, and radiation damage.

Sample charging

Emission of electrons from the surface of an insulator during X-irradiation leads to the creation of a positive surface potential since electrons from the bulk of the sample or from the sample mount cannot compensates for this loss. The effect of this positive charging is a decrease in the kinetic energy of the photoelectrons (i.e. an apparent increase in binding energy). In the case of non-monochromatic X-ray sources a compensating flux of electrons is fortuitously provided by the window of the X-ray source (generally a thin aluminium or beryllium foil) and possibly by impingement of the broad X-ray beam onto other metallic components in the sample vicinity. The overall result is a small equilibrium potential, which is effectively established instantaneously, of typically <10eV (dependent on instrument configuration, take-off angle and X-ray source operating conditions for a given polymer).

In the case of monochromated X-ray sources the situation is much more serious. Firstly, the X-rays are generated remote from the sample. This means that a source of compensating electrons has to be introduced deliberately, generally from a high current, low energy electron source. This is usually referred to as an electron ‘flood’ gun because the beam is designed to cover a large area. Secondly, the X-rays are focused onto a small area and the lack of uniform irradiation can lead to differential charging of the sample. Furthermore, unless the X-ray and electron beams are close to coaxial there will be the additional problem that effective neutralisation may only be possible over a restricted range of take-off angle.

Information

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Book purchase

Temporarily unavailable

Save book to Kindle

To save this book to your Kindle, first ensure no-reply@cambridge.org is added to your Approved Personal Document E-mail List under your Personal Document Settings on the Manage Your Content and Devices page of your Amazon account. Then enter the ‘name’ part of your Kindle email address below. Find out more about saving to your Kindle.

Note you can select to save to either the @free.kindle.com or @kindle.com variations. ‘@free.kindle.com’ emails are free but can only be saved to your device when it is connected to wi-fi. ‘@kindle.com’ emails can be delivered even when you are not connected to wi-fi, but note that service fees apply.

Find out more about the Kindle Personal Document Service.

  • Information from polymer XPS
  • D. Briggs, Wilton Materials Research Centre, ICI Chemicals and Polymers Ltd
  • Book: Surface Analysis of Polymers by XPS and Static SIMS
  • Online publication: 08 October 2009
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525261.004
Available formats
×

Save book to Dropbox

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Dropbox.

  • Information from polymer XPS
  • D. Briggs, Wilton Materials Research Centre, ICI Chemicals and Polymers Ltd
  • Book: Surface Analysis of Polymers by XPS and Static SIMS
  • Online publication: 08 October 2009
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525261.004
Available formats
×

Save book to Google Drive

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Google Drive.

  • Information from polymer XPS
  • D. Briggs, Wilton Materials Research Centre, ICI Chemicals and Polymers Ltd
  • Book: Surface Analysis of Polymers by XPS and Static SIMS
  • Online publication: 08 October 2009
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525261.004
Available formats
×