Chapter 5 - Information from SSIMS

Published online by Cambridge University Press:  08 October 2009

D. Briggs
Affiliation:
Wilton Materials Research Centre, ICI Chemicals and Polymers Ltd
Get access

Summary

There are inherent differences between the spectral features relating to polymers per se and the (usually) lower molecular weight species, such as contaminants and additives, which are often detected on polymer surfaces. It is, therefore, convenient to discuss these separately. Cationisation, deliberately induced or otherwise, leads to major variations in spectra from either class of material which are further discussed in Section 5.4. The identification of the atomic species from which either polymers or ‘small’ molecules are composed is, however, fairly straightforward.

Elemental identification

Most of the important elements in polymer surface analysis can be identified directly from peaks at the appropriate atomic masses. For high mass resolution instruments (i.e. m/Δm>3000) elemental peaks are resolved from interfering organic cluster ions and identification is either by exact mass measurement or by detection of the expected isotopic abundancies. This is particularly important for the detection of low concentration metallic species which give positive ion peaks of lower intensity than the interfering organic fragment ions from either the polymer or other organic species at the surface. Fig. 5.1 illustrates the detection of zinc at the surface of a poly(styrene) sample; this would not be possible with a low mass resolution instrument. The great majority of metals give exclusively positive ions under SSIMS conditions. The most electropositive elements, i.e. the alkali and alkali earth metals, give particularly high positive ion yields. Conversely, the electronegative elements, i.e. oxygen, fluorine, chlorine, bromine and iodine, give intense negative ion signals. Hydrogen gives both H+ and H- in high yield.

Carbon is detected as C-, although the accompanying CH- is always more intense. Nitrogen is not detected via an elemental peak. If the concentration is high enough (particularly if a low resolution instrument is used) the CN- and/or CNO- peaks are readily observed.

Information

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Book purchase

Temporarily unavailable

Save book to Kindle

To save this book to your Kindle, first ensure no-reply@cambridge.org is added to your Approved Personal Document E-mail List under your Personal Document Settings on the Manage Your Content and Devices page of your Amazon account. Then enter the ‘name’ part of your Kindle email address below. Find out more about saving to your Kindle.

Note you can select to save to either the @free.kindle.com or @kindle.com variations. ‘@free.kindle.com’ emails are free but can only be saved to your device when it is connected to wi-fi. ‘@kindle.com’ emails can be delivered even when you are not connected to wi-fi, but note that service fees apply.

Find out more about the Kindle Personal Document Service.

  • Information from SSIMS
  • D. Briggs, Wilton Materials Research Centre, ICI Chemicals and Polymers Ltd
  • Book: Surface Analysis of Polymers by XPS and Static SIMS
  • Online publication: 08 October 2009
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525261.006
Available formats
×

Save book to Dropbox

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Dropbox.

  • Information from SSIMS
  • D. Briggs, Wilton Materials Research Centre, ICI Chemicals and Polymers Ltd
  • Book: Surface Analysis of Polymers by XPS and Static SIMS
  • Online publication: 08 October 2009
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525261.006
Available formats
×

Save book to Google Drive

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Google Drive.

  • Information from SSIMS
  • D. Briggs, Wilton Materials Research Centre, ICI Chemicals and Polymers Ltd
  • Book: Surface Analysis of Polymers by XPS and Static SIMS
  • Online publication: 08 October 2009
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525261.006
Available formats
×